Material Notes:
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materials. It features exceptional shear strength and adhesion to high surface energy (HSE) plastics and metal surfaces.Designed to meet the performance requirements of most membrane keyboards. Outstanding resistance to temperature extremes, chemicals and humidity. Also resists oozing, lifting and separation of switch layers. All products feature 2 mils of 200MP on each sideInformation provided by 3M
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Polyester
50.8 microns
2.00 mil
Adhesive
50.8 microns
2.00 mil
Adhesive
Mechanical Properties Metric English Comments
Shear Strength 0.469 MPa
68.0 psi
Cohesion Dynamic, PET/Stainless Steel; ASTM D1002
0.483 MPa
70.0 psi
Cohesion Dynamic, PET/Polycarbonate; ASTM D1002
Peel Strength 0.4602 kN/m
2.625 pli
90° Peel, PET/Aluminum, Initial (20 mins); ASTM D3330
0.53686 kN/m
3.0625 pli
90° Peel, PET/PET, Initial (20 mins); ASTM D3330
0.5478 kN/m
3.125 pli
90° Peel, PET/Polycarbonate, Initial (20 mins); ASTM D3330
0.701 kN/m
4.00 pli
90° Peel, PET/Stainless Steel, Initial (20 mins); ASTM D3330
0.73407 kN/m
4.1875 pli
90° Peel, PET/PET, 72 hrs at RT; ASTM D3330
0.789 kN/m
4.50 pli
90° Peel, PET/Polycarbonate, 72 hrs at RT; ASTM D3330
0.920 kN/m
5.25 pli
90° Peel, PET/Aluminum, 72 hrs at RT; ASTM D3330
0.920 kN/m
5.25 pli
90° Peel, PET/Polycarbonate, 72 hrs at 70°C; ASTM D3330
1.23 kN/m
7.00 pli
90° Peel, PET/Stainless Steel, 72 hrs at RT; ASTM D3330
1.380 kN/m
7.875 pli
90° Peel, PET/PET, 72 hrs at 70°C; ASTM D3330
1.797 kN/m
10.25 pli
90° Peel, PET/Stainless Steel, 72 hrs at 70°C; ASTM D3330
1.84 kN/m
10.5 pli
90° Peel, PET/Aluminum, 72 hrs at 70°C0; ASTM D3330
Thermal Properties Metric English Comments
CTE, linear 6.10 µm/m-°C

@Temperature 27.0 - 175 °C
3.39 µin/in-°F

@Temperature 80.6 - 347 °F
ASTM D696
Electrical Properties Metric English Comments
Volume Resistivity 5.70e+14 ohm-cm
5.70e+14 ohm-cm
ASTM D257
Surface Resistance >= 5.60e+16 ohm
>= 5.60e+16 ohm
ASTM D257
Insulation Resistance 1.00e+13 ohm
1.00e+13 ohm
100VDC, 60 sec; Mil-I-46058C
Dielectric Constant 3.48
3.48
ASTM D150
Dielectric Strength 59.1 kV/mm
1500 kV/in
ASTM D149
Dissipation Factor 0.016
0.016
ASTM D150
Descriptive Properties Value Comments
Adhesive Type 200MP
Liner 58# PCK 4.2