Electrical Properties Metric English Comments
Dielectric Strength 59.1 kV/mm
1500 kV/in
IPC-TM-650.2.5.6.2
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg
The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a..
Dielectric Strength 59.1 kV/mm
1500 kV/in
ASTM D-149
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.015" thick)
T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele..
Dielectric Strength 59.1 kV/mm
1500 kV/in
Tra-Con Tra-Bond Ablebond 933-1.5 Moisture Resistant Encapsulant
TRA-BOND 933-1.5 electrically insulating epoxy encapsulant is formulated to provide a smooth crown over the device of wire bonds. This encapsulant provides protection from thermal and mechanical sho..
Dielectric Strength 59.1 kV/mm
1500 kV/in
ASTM D149
ExxonMobil LDPE LD 157CW Wire & Cable Low Density Polyethylene Resin
Product Description: LD 157CW is a medium density LDPE recommended for the production of Low Voltage power cable insulation, using the on-step silane cross0linking technology. The grade contains a h..
Dielectric Strength 59.1 kV/mm
1500 kV/in
500 V/sec; ASTM D149
ExxonMobil LLDPE LL 6101RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6101 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Thermal..
Dielectric Strength 59.1 kV/mm
1500 kV/in
500 V/sec; ASTM D149
ExxonMobil LLDPE LL 6101XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6101 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Thermal..
Dielectric Strength 59.1 kV/mm
1500 kV/in
ASTM D149
ExxonMobil LLDPE LL 6201RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6201 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N..
Dielectric Strength 59.1 kV/mm
1500 kV/in
ASTM D149
ExxonMobil LLDPE LL 6201XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6201 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N..
Dielectric Strength 59.1 kV/mm
1500 kV/in
500 V/sec; ASTM D149
ExxonMobil LLDPE LL 6301RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6301 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N..
Dielectric Strength 59.1 kV/mm
1500 kV/in
500 V/sec; ASTM D149
ExxonMobil LLDPE LL 6301XR Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6301 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N..
Dielectric Strength 59.1 kV/mm
1500 kV/in
ASTM D149
Arlon 514B12R006 0.006" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2116 FiberglassThis data represents typical values for the production material and should not be ..
Dielectric Strength 59.1 kV/mm
1500 kV/in
30% RH
3M Novec™ 2702 Electronic Grade Coating
3M™ Novec™ 2702 Electronic Grade Coating is designed for protection of printed circuit boards and electronic components. It is a clear, low viscosity solution of a 2 wt% fluorochemical polymer coa..
Dielectric Strength >= 59.1 kV/mm

@Thickness 0.0508 mm
>= 1500 kV/in

@Thickness 0.00200 in
Cured; ASTM D149
Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating
Room temperature curing, low modulus urethane conformal coatingAPTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the e..
Dielectric Strength >= 59.1 kV/mm

@Thickness 0.0762 mm
>= 1500 kV/in

@Thickness 0.00300 in
Cured; ASTM D149
Aptek 7503LM-PMF UV Urethane Conformal Coating
UV-cured, low modulus, shadow cures under components. Excellent adhesion without primer. Repairable. Qualified to MIL-I-46058C, types UR and AR. Castable version – UVIKOTE 7504 LM-PMF.Information p..
Dielectric Strength >= 59.1 kV/mm

@Thickness 0.0762 mm
>= 1500 kV/in

@Thickness 0.00300 in
Cured; ASTM D149
Aptek 7504LM-PMF UV Urethane Coating/Encapsulant
UV-cured,100% solids version of UVIKOTE 7503 LM-PMF. Castable/brushable viscosity for higher coating build-up. QPL listed on MIL-I-46058C, types UR an AR.Information provided by Aptek Laboratories, ..
Dielectric Strength >= 59.1 kV/mm

@Thickness 0.0762 mm
>= 1500 kV/in

@Thickness 0.00300 in
Cured; ASTM D149
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound
UVISTAKE 7205LM-PMF is a 100% solids, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic component..
Dielectric Strength >= 59.1 kV/mm

@Thickness 0.0762 mm
>= 1500 kV/in

@Thickness 0.00300 in
Cured; ASTM D149
Aptek UVISTAKE 7206 UV Curing, Urethane staking compound
UVISTAKE 7206 is a 100% solid, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic components mount..
Dielectric Strength 59.1 kV/mm
1500 kV/in
ASTM D149
3M 7945MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 59.1 kV/mm
1500 kV/in
ASTM D149
3M 7961MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 59.1 kV/mm
1500 kV/in
ASTM D149
3M 9061MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength >= 59.1 kV/mm

@Thickness 0.0762 mm
>= 1500 kV/in

@Thickness 0.00300 in
Cured; ASTM D149
Aptek 2503-A/B Low modulus urethane conformal coating
APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electronic services mounted on p..
Dielectric Strength 59.1 kV/mm
1500 kV/in
ASTM D149
3M 9045MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Dielectric Strength 59.1 kV/mm
1500 kV/in
IPC TM-650 2.5.6.2
Arlon 45N Multifunctional Epoxy Laminate and Prepreg
Arlon 45N is a tough, high Tg (175°C by DSC) multifunctional epoxy laminate and prepreg system designed for use in a variety of higher layer count MLBs. Processable using conventional FR-4 conditi..
Dielectric Strength 59.1 kV/mm
1500 kV/in
IPC TM-650 2.5.6.2
Arlon 44N Multifunctional Microdispersed Ceramic Filled Epoxy-Fiberglass Prepreg
Arlon 44N is a high resin content multifunctional (175°C) epoxy prepreg system with a proprietary microdispersed ceramic filler system. 44N is engineered for the filling of clearance holes in thi..