Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.5478 kN/m | 3.125 pli | Adhesion to Steel; ASTM D3330 |
3M 3382 HVAC Construction Foil/PET laminate. Tear resistance. Roof and gutter repair tape.Information provided by 3M |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Stainless Steel, Adhesion; ASTM D3330 |
3M 411DL Flexomount™ Solid Printing Tapes 3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Steel, 180° Peel, 72 hr dwell, Faceside; ASTM D3330 |
3M 9415PC Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Steel, 180° Peel, 72 hr dwell, Faceside; ASTM D3330 |
3M 9416 Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Rigid PVC, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9482PC Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | to Steel, Initial at RT |
3M 9738R Double Coated Splicing Tape 3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 3732 High Performance Printed Box Sealing Tape Scotch® Box Sealing Tape 3732 is a high performance packaging tape used for box sealing, splicing, recouperage, and other demanding packaging applications. This product has a heavy-duty, conformabl.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 824 Pouch Tape Scotch® Pouch Tape 824 is a pressure-sensitive tape with a bright, orange boarder on all four edges, and a non-tack “see-through” central rectangle, which provides a quick, simple, highly visible.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 825 Pouch Tape Scotch® Pouch Tape 825 is a pressure-sensitive tape with a bright, orange boarder on all four edges, and a non-tack “see-through” central rectangle, which provides a quick, simple, highly visible.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Adhesion to Steel; ASTM D3330 |
3M ScotchPad™ 830 Pouch Tape Pads 3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is cl.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Stainless Steel, 180° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7120 Performance Paper Label Material 3M™ Label Materials 7120 and 7122 latex impregnated paper with 3M™ 400 and 320 adhesives offer good conformability to curved surfaces and resistance to staining and moisture. Label Material 7120 h.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7880 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Material 7880 is a 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for traditional.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7883 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Materials 7883 is a 3.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for tradition.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Finely Textured Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Finely Textured Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7931 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | 90° Peel, PET/Stainless Steel, Initial (20 mins); ASTM D3330 |
3M 7953MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 828 Custom Printed Pouch Tape A pressure sensitive pouch tape printed tape with a company logo or design in a variety of colors. This tape features a clear, non-tacky window for displaying documents and it offers a strong Scotch.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | 90° Peel, PET/Stainless Steel, Initial (20 mins); ASTM D3330 |
3M 7956MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Non-linered side-Polyester, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1920 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |