Material Notes:
3M™ Double Coated Tapes with 3M™ Adhesive 375 provides a high level of adhesive peel and shear performance. The adhesive system used on these products provides good adhesion to both high and low surface energy substrates. The excellent initial tack ensures that a bond of good integrity is achieved soon after applicationInformation provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Liner Caliper
259 microns
10.2 mil
Total Thickness
Mechanical Properties Metric English Comments
Peel Strength 0.8984 kN/m
5.125 pli
HDPE, 180° Peel, 2-mil Al Backing; ASTM D3330
1.3038 kN/m
7.4375 pli
High Pressure Laminate, 180° Peel, 2-mil Al Backing; ASTM D3330
1.556 kN/m
8.875 pli
Stainless Steel, 180° Peel, 2-mil Al Backing; ASTM D3330
1.600 kN/m
9.125 pli
Polycarbonate, 180° Peel, 2-mil Al Backing; ASTM D3330
1.600 kN/m
9.125 pli
ABS, 180° Peel, 2-mil Al Backing; ASTM D3330
1.797 kN/m
10.25 pli
Glass, 180° Peel, 2-mil Al Backing; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 70.0 °C
158 °F
Continuous
85.0 °C
185 °F
Short Term
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Carrier PVC 1.5 mils
Adhesive Type Modified Acrylic
Appearance White
White Paper (Glassine) with Green 3M Logo