Mechanical Properties Metric English Comments
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
3M 9472 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
3M 9672 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Peel Strength 0.8984 kN/m
5.125 pli
Polycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
3M 9674 Adhesive Transfer Tapes with Adhesive 300
3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f..
Peel Strength 0.8984 kN/m
5.125 pli
Polypropylene, 180° Peel, Conditioned 3 day dwell at RT; ASTM D3330
3M 7620/7890 White Vinyl Label Material
3M™ White Vinyl Label Material 7620 / 7890 is a rigid, gloss vinyl film with excellent durability. This label material utilizes 3M™ High Strength Acrylic Adhesive 300, which has excellent quick ta..
Peel Strength 0.8984 kN/m
5.125 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
3M 7904 Screen Printable Sheet Vinyl Label Material
3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili..
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
90° Peel, PET/Stainless Steel, 72 hrs at 70°C; ASTM D3330
3M 7993MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
Peel Strength 0.8984 kN/m
5.125 pli
to stainless steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330
3M 9009 Double Coated Tapes with Adhesive 300
3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides..
Peel Strength 0.8984 kN/m
5.125 pli
to stainless steel, 90°, 72 hr RT; ASTM D3330
3M 9039 Double Coated Tapes with Adhesive 300
3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides..
Peel Strength 0.8984 kN/m
5.125 pli
HDPE, 180° Peel, 2-mil Al Backing; ASTM D3330
3M 9087 High Performance Double Coated Tapes with Adhesive 375
3M™ Double Coated Tapes with 3M™ Adhesive 375 provides a high level of adhesive peel and shear performance. The adhesive system used on these products provides good adhesion to both high and low s..
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
Stainless Steel, 90°, 72 hr RT; ASTM D3330
3M 9579 Double Coated Tape with Adhesive 760
3M™ Double Coated Tape 9579 with 3M™ Adhesive 760 is a high-tack, hand-tearable, double coated film tape with a pressure sensitive adhesive on each side of the carrier. The medium firm adhesive fe..
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
to Stainless Steel, 90° peel, 2 mil aluminum foil backing, 72 hour RT
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
Peel Strength 0.8984 kN/m
5.125 pli
to Polyester, 90°, 2 mil Al foil, 72 hr RT; ASTM D3330
3M 9589 Double Coated Tapes with Adhesive 700 Series
3M™ Double Coated Tapes with 3M™ Adhesive 700 Series feature a high tack synthetic rubber adhesive which provides excellent quick stick or initial adhesion and bonds together a wide variety of mat..