3M ATG 928 Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name ATG
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M ATG 928 Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
0.002 in. (0.05 mm) thick high-tack/low-tack double coated tapeInformation provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Tape
152 microns
6.00 mil
Release Liner
Descriptive Properties Value Comments
Adhesive Type 400/1000
Appearance White
Liner White Paper polycoated kraft