Material Notes:
3M™ Dyneon™ Fluoroplastic Granules THV 221GZ is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provides a balance of low temperature processing, low flammability, thermal stability, and melt processability. It can be used to prepare extruded films, tubes, profiles, and wire coatings. It is useful for applications that require a high level of flexibility, transparency, low temperature fusion or bonding capability with moderate chemical resistance. Laminated films of this product exhibit excellent weatherability and good anti-soiling properties. This product can be E-beam cured without the need of pro-rads to improve its high temperature capability with minimal loss of flexibility. Process at relatively low temperatures compared to other fluoroplastics and may not require the same level of corrosion resistant equipment as that used with higher melting fluoroplastics. However, it should be remembered that THV is a fluoroplastic and should be treated accordingly.Features and Benefits:Ultra flexible grade of THVProcessing profile allows coprocessing with olefinic plastics and hydrocarbon elastomersExcellent chemical and permeation resistanceHigh transparencyLow flammabilityBondable to itself and other substrates (for multi-layer constructions)E-beam crosslinkableInformation provided by the Dyneon division of 3M.
Physical Properties Metric English Comments
Specific Gravity 1.93 g/cc
1.93 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 5.00 kg,
Temperature 265 °C
20 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
film; ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Flexural Modulus 0.0800 GPa
11.6 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 115 °C
239 °F
ASTM D4591
Oxygen Index 65 %
65 %
ASTM D2863
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified