3M F-9755PC Adhesive Transfer Tapes with 420 Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M F-9755PC Adhesive Transfer Tapes with 420 Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2.0 mil, 420 high tack acrylic adhesive with 4.2 mil, 58 lb polycoated kraft paper liner.Features:2.0 mil adhesive transfer tape. 58 lb polycoated kraft paper liner. 420 Acrylic AdhesiveHigh tack adhesive. Can be applied in temperatures as low as 32 degrees FahrenheitBonds gaskets and foams. Bonds polycarbonate instrument panels.General Industrial Applications, Automotive, TransportationThis is good for adhering, joining, affixing, bonding, mounting, holding, and attaching dissimilar materials. Plastic film lamination bonding, splicing, foam laminating, Gasket and foam attachmentInformation provided by 3M
Physical Properties Metric English Comments
Thickness 102 microns
4.00 mil
Release Liner
127 microns
5.00 mil
Tape Only
Mechanical Properties Metric English Comments
Peel Strength 0.60259 kN/m
3.4375 pli
to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Long term
323 °C
613 °F
Short term
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 420
Appearance Clear
Liner Moisture Resistant Tan Paper