Material Notes:
A warm applied, moisture-curing polyurethane adhesive for wood working, laminating and plastic component assembly.Low viscosity. Long open time. Thin glue lines. Very high strength to wood. Bonds selected plastics.Information provided by 3M
Physical Properties Metric English Comments
Viscosity 3000 cP
3000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Tensile Strength, Ultimate 27.6 MPa
4000 psi
Elongation at Break 625 %
625 %
Modulus of Elasticity 0.0669 GPa
9.70 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F