Material Notes:
3M Heat Shrink Tubing MW is a semi-rigid, 110°C heat-shrinkable polyolefin tubing that is a co-extruded and selectively cross-linked to provide an integral, meltable inner wall. When heated in excess of 135°C, the inner meltable wall of the tubing is simultaneously softened and forced by the shrink action into intimate contact with all underlying surfaces, interstices and small voids. Upon cooling, the MW tubing provides a tough protective and insulating barrier, highly resistant to penetration by moisture and the introduction of chemicals and solvents. Adhesive reflow will occur at temperatures about 80°C.Information provided by 3M
Physical Properties Metric English Comments
Water Absorption 0.10 %
0.10 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.2 MPa
2200 psi
Elongation at Break 400 %
400 %
175 %

@Temperature 175 °C,
Time 1.21e+6 sec
175 %

@Temperature 347 °F,
Time 336 hour
Heat Aged
2% Secant Modulus 0.186 GPa
27.0 ksi
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Strength 35.4 kV/mm
900 kV/in