Material Notes:
Chemical composition above is wt%. Filament diameter is 10-12 µm.3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 and do not contain glassy phases. This allows the fibers to retain their strength at high temperatures. 3M Nextel Fiber 610 is a fine grained single-phase composition of alpha-Al2O3. It has the highest strength at room temperature. However, because it is essentially single phased, the strength decreases rapidly at high temperatures due to grain growth.Information provided by 3M Ceramic Textile and Composites.
Physical Properties Metric English Comments
Density 3.90 g/cc
0.141 lb/in³
Particle Size <= 0.50 µm
<= 0.50 µm
Crystal size
Specific Surface Area <= 0.20 m²/g
<= 0.20 m²/g
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3100 MPa

@Thickness 25.4 mm
450000 psi

@Thickness 1.00 in
filament
Modulus of Elasticity 373 GPa
54100 ksi
Filament in Tension
Thermal Properties Metric English Comments
CTE, linear 8.00 µm/m-°C

@Temperature 100 - 1100 °C
4.44 µin/in-°F

@Temperature 212 - 2010 °F
Melting Point 2000 °C
3630 °F
Optical Properties Metric English Comments
Refractive Index 1.74
1.74
Component Elements Properties Metric English Comments
Al2O3 >= 99 %
>= 99 %
Descriptive Properties Value Comments
Color Off-White
Users viewing this material also viewed the following: