Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 0.50 µm | >= 0.50 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 313 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 21.8% of partciles less than |
Old Hickory M&M Clays, Inc. Wilco-LPC Kaolin Clay Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SL.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 44% of particles less than |
Old Hickory M-33 Kentucky Ball Clay The M-33 ball clay is a carbonaceous selection that bears similarity to some clays found in the Southwestern section of England. It has a uniquely waxy type of plasticity and provides high green and.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 56% of particles less than |
Old Hickory MCB-11 Tennessee Ball Clay A clay with excellent kaolin content and virtually no carbon content. It is highly plastic with excellent fired brightness and is an excellent clay for a variety of ceramic glaze and porcelain compo.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 43% of particles less than |
Old Hickory No. 28 Kentucky Ball Clay This is a kaolin grade with exceptional plasticity, dry and green strength, and low levels of carbon content. it can be utilized in extruded or pressed ceramic formulations and is a clay particularl.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 56% of particles less than |
Old Hickory Thomas Tennessee Ball Clay Thomas clay is similar to Volunteer clay and has established an excellent history of performance in stoneware and low fire (talc base) plastic and casting formulas. The diverse combination of clays .. |
|||
Particle Size | 0.50 µm | 0.50 µm | 43% of particles less than |
Old Hickory UltraCast Slurry UC-34A Kentucky Ball Clay These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 52% of particles less than |
Old Hickory Volunteer Tennessee Ball Clay A versatile clay selection for casting, pressing, or plastic forming process methods. It is similar to M-23 in mineralogy with slightly more organic content. Volunteer has very good plasticity and i.. |
|||
Particle Size | 0.50 - 1.0 µm | 0.50 - 1.0 µm | D<sub>50</sub> |
NYC YT3WP Y2O3 Granules |
|||
Particle Size | <= 0.50 µm | <= 0.50 µm | 400 mesh |
Hong Kun Group Zinc Borate Flame Retardant CAS No. 1332-07-6All information provided by Hongkun Group |
|||
Particle Size | 0.50 µm | 0.50 µm | 28% finer than |
Imerys Allenâ„¢ Kaolin Allen is an intermediate-grained kaolin suitable for use as a filler and pigment in a wide variety of industrial applications such as soft rubber, plastics, ceiling tile, adhesives and paper product.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 72% finer than |
Imerys Amlockâ„¢ 321 Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 72% finer than |
Imerys Bardenâ„¢ Kaolin Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 71.5% finer than |
Imerys Barnetâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 45% finer than |
Imerys Carverâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 23% finer than |
Imerys Kaolin Slurryâ„¢ Kaolin Slurry is a carefully controlled Kaolin-water suspension formulated for use in cermic castings.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 25% finer than |
Imerys Kingsleyâ„¢ Kaolin Kingsley is a coarse-grained, white firing kaolin used in the dinnerware, tile, artware and electrical porcelain industries.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 20% finer than |
Imerys KT Cast Slurryâ„¢ Kaolin KT Cast Slurry is a carefully controlled kaolin-water suspension formulated for use in ceramic operations.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 21% finer than |
Imerys KT Castâ„¢ Kaolin KT Cast is a coarse-grained, white firing kaolin that is used primarily in casting bodies based on its fast casting and exceptional deflocculation characteristics.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 30% finer than |
Imerys KT-Cast/Rogersâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 72% finer than |
Imerys Mercapâ„¢ 100 Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 10% |
Minelco UltraCarb LH3 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | 0.50 µm | 0.50 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade BF 17 Silicon Carbide, SiC Beta SiC for sintering.Sliding bearingsSeal ringsWear partsKiln furniture, crucibles, heating elements, burner nozzles, heat exchangersSemiconductor handling partsComponents for wafer processing (su.. |
|||
Particle Size | 0.50 µm | 0.50 µm | |
Shin-Etsu Silicones X-52-2328 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 0.50 - 1.0 µm | 0.50 - 1.0 µm | D50 Sedigraph |
Solvay Polishing Opaline™ Description: Polishing OPALINE® is a high quality cerium oxide powder developed high precision polishing. It has an excellent surface quality, very low roughness, and has quality consistency. The.. |
|||
Particle Size | 0.50 - 25 µm | 0.50 - 25 µm | PSD (d<sub>50</sub> |
Terio Corporation TZY-10 Yttria Stabilized Zirconia Information provided by TERIO Corporation. |
|||
Particle Size | 0.50 - 25 µm | 0.50 - 25 µm | PSD (d<sub>50</sub> |
Terio Corporation TZY-4 Yttria Stabilized Zirconia Information provided by TERIO Corporation. |
|||
Particle Size | 0.50 µm | 0.50 µm | TiB<sub>2</sub> Crystal Size |
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (.. |
|||
Particle Size | <= 0.50 µm | <= 0.50 µm | Crystal size |
3M Nextel™ 720 Composite Ceramic Fiber Chemical composition above is wt%. Filament diameter is 10-12 µm.3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 .. |
|||
Particle Size | 0.50 µm | 0.50 µm | 55% of particles less than |
Old Hickory TI-21 Tennessee Ball Clay TI-21 is a very low carbon content clay specifically designed for plastic forming methods. It has excellent oxidation qualities particularly for dense volume stoneware or vitreous ceramic pieces. Th.. |