3M Scotch™ 130C Linerless Rubber Splicing Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch™ 130C Linerless Rubber Splicing Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch™ Linerless Rubber Splicing Tape 130C is a high conformable, linerless, ethylene rubber (EPR), high-voltage insulating tape, formulated to provide excellent thermal dissipation of splice heat. The tape is designed for use in splicing and terminating wires and cables. Rated up to 90°C continuous operating temperatures and short-term 130°C overload service. The tape has excellent physical and electrical properties, which provide immediate moisture seals and void-free build-ups. The product can be used for low and high-voltage (through 69 kV) applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 762 microns
30.0 mil
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.72 MPa
249 psi
ASTM D4325
Elongation at Break 850 %
850 %
ASTM D4325
Thermal Properties Metric English Comments
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
ASTM C518
Maximum Service Temperature, Air 90.0 °C
194 °F
Continuous
130 °C
266 °F
Emergency Overload
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Aged 96 hrs at 96% RH; ASTM D4325
>= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Original; ASTM D4325
Dielectric Constant 3.5

@Frequency 60.0 Hz,
Temperature 23.0 °C
3.5

@Frequency 60.0 Hz,
Temperature 73.4 °F
1200V; ASTM D4325
3.6

@Frequency 60.0 Hz,
Temperature 90.0 °C
3.6

@Frequency 60.0 Hz,
Temperature 194 °F
1200V; ASTM D4325
Dielectric Strength 28.7 kV/mm
730 kV/in
96 hrs at 96% RH; ASTM D4325
29.5 kV/mm
750 kV/in
Original; ASTM D4325
29.5 kV/mm
750 kV/in
24 hrs in water; ASTM D4325
Dissipation Factor 0.70

@Frequency 60.0 Hz,
Temperature 23.0 °C
0.70

@Frequency 60.0 Hz,
Temperature 73.4 °F
1200V; ASTM D4325
Descriptive Properties Value Comments
Appearance Black