3M Scotch-Weld™ 2086 One-Part Epoxy Adhesives and Metal Primer

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 2086 One-Part Epoxy Adhesives and Metal Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Temperature strength and High ViscosityInformation provided by 3M
Mechanical Properties Metric English Comments
Shear Strength 15.2 MPa

@Temperature 121 °C
2200 psi

@Temperature 250 °F
Overlap
20.7 MPa

@Temperature -55.0 °C
3000 psi

@Temperature -67.0 °F
Overlap
34.5 MPa

@Temperature 24.0 °C
5000 psi

@Temperature 75.2 °F
Overlap
34.5 MPa

@Temperature 82.0 °C
5000 psi

@Temperature 180 °F
Overlap
Peel Strength 0.877 kN/m
5.00 pli
T-Peel
Processing Properties Metric English Comments
Cure Time 60.0 min

@Pressure 0.0689 MPa,
Temperature 177 °C
1.00 hour

@Pressure 10.0 psi,
Temperature 351 °F