Material Notes:
3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a paste consistency epoxy adhesive designed for bonding metals and many high temperature plastics such as fiberglass reinforced plastic, polyester, and phenolicsInformation provided by 3M
Physical Properties Metric English Comments
Viscosity 15 - 30 cP
15 - 30 cP
Mechanical Properties Metric English Comments
Hardness, Shore D >= 88
>= 88
Tensile Strength, Ultimate 55.2 MPa
8000 psi
Elongation at Break 1.0 %
1.0 %
Modulus of Elasticity 5.52 GPa
800 ksi
Shear Strength 6.21 MPa

@Temperature 177 °C
900 psi

@Temperature 351 °F
Aluminum Overlap
13.8 MPa

@Temperature -53.0 °C
2000 psi

@Temperature -63.4 °F
Aluminum Overlap
13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Aluminum Overlap
17.2 MPa

@Temperature 121 °C
2500 psi

@Temperature 250 °F
Aluminum Overlap
17.2 MPa

@Temperature 149 °C
2500 psi

@Temperature 300 °F
Aluminum Overlap
20.7 MPa

@Temperature 82.0 °C
3000 psi

@Temperature 180 °F
Aluminum Overlap
Thermal Properties Metric English Comments
CTE, linear 48.0 µm/m-°C

@Temperature 0.000 - 80.0 °C
26.7 µin/in-°F

@Temperature 32.0 - 176 °F
Thermal Conductivity 0.327 W/m-K
2.27 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Volume Resistivity 9.40e+13 ohm-cm
9.40e+13 ohm-cm
Surface Resistance 1.10e+17 ohm
1.10e+17 ohm
Dielectric Constant 6.2

@Temperature 23.0 °C
6.2

@Temperature 73.4 °F
ASTM D150
7.6

@Temperature 60.0 °C
7.6

@Temperature 140 °F
ASTM D150
7.8

@Temperature 90.0 °C
7.8

@Temperature 194 °F
ASTM D150
8.0

@Temperature 104 °C
8.0

@Temperature 219 °F
ASTM D150
Dielectric Strength 13.7 kV/mm

@Thickness 0.965 mm
347 kV/in

@Thickness 0.0380 in
Dissipation Factor 0.021

@Temperature 23.0 °C
0.021

@Temperature 73.4 °F
0.023

@Temperature 60.0 °C
0.023

@Temperature 140 °F
0.025

@Temperature 90.0 °C
0.025

@Temperature 194 °F
0.025

@Temperature 104 °C
0.025

@Temperature 219 °F
Arc Resistance 119 sec
119 sec
Descriptive Properties Value Comments
Appearance Gray
Users viewing this material also viewed the following: