3M Scotch-Weld™ 3797 Hot Melt Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 3797 Hot Melt Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High ball and ring; Low viscosity and Good for electrical pottingInformation provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity 2650 cP

@Temperature 191 °C
2650 cP

@Temperature 375 °F
Mechanical Properties Metric English Comments
Shear Strength 2.41 MPa
350 psi
On Douglas Fir
Peel Strength 1.75 kN/m
10.0 pli
on canvas
Thermal Properties Metric English Comments
Flammability, UL94 V-2
V-2
Ring & Ball Softening Point 151 °C
304 °F
ASTM E28-99