3M Scotch-Weld™ CA5 Instant Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ CA5 Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity, slower setting version of CA4 for filling gaps. Meets CID A-A-3097, Type II, Class 3.Information provided by 3M
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 2000 cP
2000 cP
Mechanical Properties Metric English Comments
Shear Strength 0.241 MPa
35.0 psi
Overlap, Nitrile Rubber; ASTM D1002-64
0.379 MPa
55.0 psi
Overlap, Neoprene Rubber; ASTM D1002-64
4.48 MPa
650 psi
Overlap, Aluminum; ASTM D1002-64
5.52 MPa
800 psi
Overlap, ABS; ASTM D1002-64
5.52 MPa
800 psi
Overlap, Rigid PVC; ASTM D1002-64
17.2 MPa
2500 psi
Overlap, Steel; ASTM D1002-64
Peel Strength 0.175 - 0.351 kN/m
1.00 - 2.00 pli
T-Peel
Processing Properties Metric English Comments
Cure Time 0.250 - 1.00 min
0.00417 - 0.0167 hour
Descriptive Properties Value Comments
Appearance Clear