Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 4.48 MPa @Treatment Temp. 21.0 °C, Time 86400 sec |
650 psi @Treatment Temp. 69.8 °F, Time 24.0 hour |
Lap |
Parker Chomerics CHO-BOND 584-29 Conductive Adhesive Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m.. |
|||
Shear Strength | >= 4.48 MPa | >= 650 psi | |
Parker Chomerics CHO-BOND 589-29 Conductive Epoxy Low cost, highly conductive adhesive system which combines the strong adhesion characteristics of an epoxy with the superior conductivity of silver. CHO-BOND 589-29 adhesive meets the most exacting .. |
|||
Shear Strength | 4.48 - 35.2 MPa | 650 - 5100 psi | Average value: 14.2 MPa Grade Count:58 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Shear Strength | >= 4.48 MPa | >= 650 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR III 1/4-5052-.004 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 4.48 MPa | 650 psi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® HRP - 3/16 - 7.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | >= 4.48 MPa | >= 650 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.004 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 4.48 MPa | 650 psi | Overlap, Aluminum; ASTM D1002-64 |
3M Scotch-Weld™ CA5 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity, slower setting version of CA4 for filling gaps. Meets CID A-A-3097, Type II, Clas.. |
|||
Shear Strength | 4.48 MPa | 650 psi | Overlap, ABS, Adhesive/Cohesive Failure |
3M Scotch-Weld™ DP810NS Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 4.48 MPa | 650 psi | Tensile Shear Adhesion, on a grit blasted steel |
3M Scotchkote™ SG 527 Epoxy Metal Repair Scotchkote Epoxy Metal Repair SG 527 is a specially packaged rapid curing synthetic metal repair compound for on site repairs to metal components such as leaking pipes, tanks, ducts, and radiators.P.. |
|||
Shear Strength | 4.48 MPa | 650 psi | Overlap, Glass (3/16" thick), Substrate Failure |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 4.48 MPa @Temperature 149 °C |
650 psi @Temperature 300 °F |
Etched Aluminum Overlap |
3M Scotch-Weld™ EC-1386 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M |
|||
Shear Strength | 4.48 MPa | 650 psi | Overlap, Wood, Fir |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |
|||
Shear Strength | 4.48 MPa | 650 psi | Overlap, PVC |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |