3M Scotch-Weld™ TL42 Threadlocker Anaerobic Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ TL42 Threadlocker Anaerobic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Threadlocker Anaerobic Adhesives are one-component anaerobic adhesives that cure and seal threaded assemblies that meet a wide range of applications to prevent vibration loosening and/or leakage. All products provide excellent vibration, corrosion, and shock resistance. Engineered to provide different strengths, temperatures, nut/bolt sizes, and other requirements, some threadlockers allow removal and meet various selections depending on the specific application. TL42 is a general purpose, removable with hand tools, medium strength threadlocker ideal for machine tool access bolts, and hydraulic system bolts. It can also be used on gear box/driveshaft bolts, bearing cover cap screws, countersunk screws, and conveyor roller bolts.Information provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity 800 - 1600 cP
800 - 1600 cP
RVT #2 sp @ 20 rpm
Processing Properties Metric English Comments
Cure Time <= 5.00 min
<= 0.0833 hour
Fixture Time with Activator
<= 20.0 min
<= 0.333 hour
Fixture Time
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Blue