3M ScotchPad™ 830 Pouch Tape Pads

Category Polymer , Adhesive
Manufacturer 3M
Trade Name ScotchPad™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M ScotchPad™ 830 Pouch Tape Pads.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is clear and becomes a “see-through” window. Each piece to tape is coupled with a strip of liner material for easy handling and application without the need of a dispenser. The product provides a quick, simple, and secure method of attaching and protecting packing lists and other documents on a wide range of shipping containers. With the liner left in place, the product many be used as an open-ended pouch, allowing work tickets, inventory lists, and other shipping documents to be inserted or removed as necessary.Information provided by 3M
Physical Properties Metric English Comments
Thickness 63.5 microns
2.50 mil
ASTM D3652
Mechanical Properties Metric English Comments
Elongation at Break 160 %
160 %
ASTM D3759
Peel Strength 0.5478 kN/m
3.125 pli
Adhesion to Steel; ASTM D3330
Film Tensile Strength at Break, MD 7.95 MPa
1150 psi
ASTM D3759
Film Tensile Strength at Break, TD 15.9 MPa
2310 psi
ASTM D3759
Descriptive Properties Value Comments
Adhesive Type Pressure Sensitive Rubber Resin
Appearance Transparent