Material Notes:
DescriptionCP 812 is a linear medium-density polyethylene resin with excellent molding characteristics and good low temperature impact. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.935 g/cc
0.935 g/cc
ASTM D792
Melt Index of Compound 5.0 g/10 min
5.0 g/10 min
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.8 MPa
2150 psi
ASTM D638
Elongation at Break 150 %
150 %
ASTM D638
Flexural Modulus 0.552 GPa
80.0 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Falling Dart Impact 65.1 J

@Temperature -40.0 °C
48.0 ft-lb

@Temperature -40.0 °F
Tear Strength 140.24 kN/m
800.21 pli
ASTM D624