DescriptionFormion® FI 131E is an adhesive grade extrusion product. It has been formulated to provide adhesion as a tie layer or resin modifier to bond Ionomer to polar and non polar substances, such as impact polypropylene, Polystyrene, Polyurethane, Polycarbonate and certain polyesters. ApplicationFormion® FI 131E is targeted for exterior or interior laminates in film, sheet extrusion and blow molding applications and adhesive bonding to textiles.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ISO 1183/1
Melt Index of Compound 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
20 g/10 min

@Load 5.00 kg,
Temperature 230 °C
20 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
15 sec delay; ISO 868
Tensile Strength, Ultimate 35.0 MPa
5080 psi
at max load; ISO 527
Tensile Strength, Yield 50.0 MPa

@Strain 50.0 %
7250 psi

@Strain 50.0 %
ISO 527
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -55.0 °C
-67.0 °F