Material Notes:
DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability .Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ISO 1183/1
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
15 sec delay; ISO 868
Tensile Strength at Break 4.20 MPa
609 psi
ISO 527
Tensile Strength, Yield 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
ISO 527
Elongation at Break >= 350 %
>= 350 %
ISO 527
Tear Strength 22.3 kN/m
127 pli
ISO 34/1
Descriptive Properties Value Comments
Colorfastness/Weatherability 1240 Delta E (kJ/m^2)
SAE J1885