Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 377 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.60 MPa
377 psi
M100
3M Dyneon™ Fluorel™ FE-5730Q Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69.2%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 69.2% F grade terpolymer with good pe..
Tensile Strength, Yield 2.60 - 72.2 MPa
377 - 10500 psi
Average value: 23.7 MPa Grade Count:77
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Tensile Strength, Yield 2.60 MPa
377 psi
At 100% elongation, across flow; ASTM D412
Advanced Elastomer Systems Santoprene® 8281-65 Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
Tensile Strength, Yield 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
ISO 527
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tensile Strength, Yield 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
ISO 527
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tensile Strength, Yield 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
ISO 527
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tensile Strength, Yield 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
ISO 527
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tensile Strength, Yield 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
ISO 527
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tensile Strength, Yield 2.60 MPa

@Strain 100 %
377 psi

@Strain 100 %
ISO 527
A. Schulman INVISION™ VX-5060UI INVISIONTMSoft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5060UI is a UV-stabilized polyolefin-based thermoplastic elastomer of 60 Shore A durometer, which has been formulated for easy moldability, soft touch, low gloss, and excell..
Tensile Strength, Yield 2.60 MPa
377 psi
ASTM D638
Arkema Group OREVAC® 9304 EVA Terpolymer
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre..
Tensile Strength, Yield 2.60 - 4.00 MPa

@Temperature 70.0 - 100 °C
377 - 580 psi

@Temperature 158 - 212 °F
Average value: 3.43 MPa Grade Count:1
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Copyright © lookpolymers.com All Rights Reserved