Material Notes:
DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Melt Flow 14 g/10 min
14 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Strength 34.0 MPa
4930 psi
ASTM D790
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256
Users viewing this material also viewed the following: