Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.47 GPa | 213 ksi | |
Plastcom SLOVALEN PQ 83 T 20 PP, 20% mineral filling FeaturesModified PP for injection moulding with the content of 20% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased .. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | Tangent; 1.3 mm/min; ASTM D790 |
Mytex Polymers AS33LW Polypropylene, Rubber modified, Talc filled, Compounded Description: AS33LW is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and good .. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP553P Fiber (Staple) Grade Polypropylene Moplen HP553P is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP553P is a homopolymer typically used by customers in high speed p.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP557G Stretch Grade Polypropylene Moplen HP557G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP557G is a homopolymer suitable for high strength rope, container .. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP562S Fiber (Spunbond) Grade Polypropylene Moplen HP562S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562S is a homopolymer particularly suitable f.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen EP641P Injection Molding Grade Polypropylene Moplen EP641P is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP641P is a block copolymer suitable for injection molding of c.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 99416 with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Homopolymer; Blow Molding, Sheeting & Profile Extrusion ResinCharacteristics: High Stiffness, Good Impact Resistance, Very Low Odor & Taste Transfer, Designated for Uniloy Blowmol.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic
(discontinued **) Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene B200P PP B200P Applications: Industrial pipesCharacteristics: Chemical resistanceInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene B201Y PP B201Y Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:Low smellFormabilityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene F400 PP F400 Film Grade HomopolymerApplications: OPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene HJ340 PP HJ340 Impact CopolymerApplications:Corrugated sheetThick board (tank, etc…)Characteristics:High impactHigh stiffnessLow warpageInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | 1% Secant; ASTM D790 |
Flint Hills P4C6Z-022 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills Res.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene J945 PP J945 Injection Impact CopolymerApplications: Very large articles:Washing M/C partsIndustrial applianceCharacteristics:High flowabilityHigh stiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene S905 PP S905 Fiber Grade HomopolymerApplications: SpunboundCharacteristics:High flowabilityProcessabilityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D760 |
LG Chemical SEETEC H7411 Polypropylene, Homopolymer Features: Seetec H7411 is designed for the extrusion of continuous filament (CF) and staple fibers. This grade is characterized by high tenacity from narrow molecular weight distribution (MWD) and U.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene J742S PP J742S Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corpora.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY 93000LTH Acrylic LNP* STAT-LOY* 93000LTH is a compound based on Acrylic resin. Added features of this material include: Antistatic, Transparent and Formulation Locked. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear. |
|||
Flexural Modulus | 1.47 GPa @Thickness 3.20 mm |
213 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SH 2157 High Impact Polystyrene Characteristics Excellent ESCR properties Good formability Processing ExtrusionApplications Refrigerator door and cabinet liners Dairy containers Ice cream cups, plates and bowlsMaterial Status: .. |
|||
Flexural Modulus | 1.47 GPa @Thickness 3.20 mm |
213 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 6520 Permanent Antistatic Polystyrene Characteristics No sloughing Fully colorable Meets MIL-PRF-81705D static decay specification Functions even in low humidity levels Processing Injection molding Extrusion & Forming Applications C.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H6430BM High Density Polyethylene Blow Molding Key Characteristics:Excellent stiffnessGood processabilityOdorlessSafe for food contactGood printabilityRecommended Applications:Bottles for drinking water, fruit juice, soft drink, milkAutomotive p.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H6670B High Density Polyethylene Film Key Characteristics:High flowExcellent processabilityHigh stiffnessOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for drinking water, fruit juice, soft drink, milkI.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Tipco Tipcolene® FPC 10 PPC - 10% Calcium Carbonate Reinforced Polypropylene Copolymer 10% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, 15% Milled Glass Filled, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Braskem H 103 Injection Molding Polypropylene Applications: Thin-walled parts and easy mould filling; food and cosmetic packing; toys and household; sealed closures. Information provided by Braskem |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |