A. Schulman POLYFORT™ FXP 1943 CaC03 and Glass Fiber Hybrid Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer A. Schulman, Inc.
Trade Name POLYFORT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FXP 1943 CaC03 and Glass Fiber Hybrid Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FXP 1943 is a 20% CAC03 and glass fiber hybrid copolymer polypropylene product. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 54.0 MPa
7830 psi
ASTM D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ASTM D648