A. Schulman POLYFORT™ PP 3045

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer A. Schulman, Inc.
Trade Name POLYFORT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ PP 3045.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D792
Melt Flow 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648