Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10641 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10641 is characterized by high fluidity with good mechanical prope.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 12642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 12642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 70 g/10 min and good mechanical properties.Polypropylene PPC 10641 has been developed for high s.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 3666 Polypropylene, Heterophasic Copolymer, Extrusion Polypropylene PPC 3666 is a heterophasic copolymer with a Melt Flow index of 1.5 g/10 min. This resin offers an outstanding processability in combination with good melt strength and excellent mecha.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 5571 Polypropylene, Impact Copolymer Injection Molding TOTAL Petrochemicals Polypropylene 5571 is a high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 5571 is characterized by significantly improved impact resistance, while m.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 11012 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 11012 is a nucleated controlled-rheology antistatic homopolymer with a high melt flow index of 55 g/10 min.Polypropylene PPH 11012 is characterized by high fluidity for high speed .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape Fading Resistance TOTAL Polypropylene 3662 is formulated to resist gas fading while maintaining excellent processing stabilityProcess Stability. 3662 features excellent processability and the good.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPH 3860X Polypropylene Homopolymer, High Flow Reactor Grade for Non-Woven Fibers High Purity TOTAL Petrochemicals Polypropylene 3860X features extremely high purity for processing in micro denier fibers.Recommended Applications. 3860X is recommended for nonwoven fiber applicat.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 4069 Polypropylene Homopolymer, Fiber Polypropylene PPH 4069 is a homopolymer polypropylene with a Melt Flow index of 4 g/10 min.Polypropylene PPH 4069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 6080 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6080 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 6088 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPM H250 Polypropylene, Homopolymer Medical Grade Polypropylene PPM H250 is a narrow molecular weight distribution homopolymer with a Melt Flow Index of 25 g/10 min recommended for the manufacture of medical packaging and medical devices, to the ex.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 3045 Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 7001 Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11750 is a nucleated and controlled-rheology heterophasic copolymer with very high Melt Flow index of 50 g/10 min.Polypropylene PPC 11750 is characterized by good impact resistance.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 3150 MX5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene PPC 3150 MX5 is a high crystallinity and high impact polypropylene (HCPP) copolymer with a Melt Flow index of 15 g/10 min. The material is UV stabilized.Polypropylene PPC 3150 MX5 is .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4524WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4524WZ is a nucleated high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 4524WZ is characterized by significantly improved impact resis.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4944CWZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4944CWZ is a nucleated and controlled rheology impact copolymer with a very high Melt Flow index of 50 g/10 min.TOTAL 4944CWZ is characterized by improved stiffnes.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 5945WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5945WZ is a nucleated impact copolymer with a Melt Flow index of 80 g/10 min.TOTAL Polypropylene 5945WZ is characterized by very low warpage, improved stiffness, a.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
Braskem H 216 Fiber Extrusion Polypropylene Homopolymer Staple fibers and continuous filaments with high tenacity and fine denier; Fibers for asbestos-free roof tiles and concrete reinforcement.Information provided by Braskem. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
Braskem H 502HC Thermoforming Polypropylene Homopolymer Disposable cupware and dishware; High-stiffness parts; Hot packaging.Information provided by Braskem. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
Braskem H 503 Raffia Extrusion & Fiber Extrusion Polypropylene Homopolymer ApplicationsRaffia Extrusion: Industrial bags; Flexible containers; Curtains and covers to aviary and agriculture.Fiber Extrusion: Monofilament for ropes; Fishing nets; Cables and ropes for boats; .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.Benefits. 4170 forms tough films with high dart imp.. |