Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 7001 Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 3045 Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet TOTAL Petrochemicals Polypropylene 4252 is a 1.5 melt flow rate impact copolymer designed for improved toughness and high melt strength. This resin offers outstanding processability in combination .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 5571 Polypropylene, Impact Copolymer Injection Molding TOTAL Petrochemicals Polypropylene 5571 is a high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 5571 is characterized by significantly improved impact resistance, while m.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 5946WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5946WZ is a nucleated impact copolymer with a Melt Flow index of 75 g/10 min.TOTAL Polypropylene 5946WZ is characterized by very low warpage, improved stiffness, a.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 7652 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 7652 is a nucleated and antistatic heterophasic copolymer with a Melt Flow index of 16 g/10 min.Polypropylene PPC 7652 is a medium flow grade intended for a wide range of injection.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact Polypropylene PPC 7810 is a very high impact heterophasic copolymer with a Melt Flow index of 15 g/10 min.Polypropylene PPC 7810 has been specially developed for high impact and heavy duty applicati.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPH 3575CC Polypropylene Homopolymer, Film Grade Low Residuals TOTAL Polypropylene 3575CC utilizes the new TOTAL Polypropylene proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblo.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPH 3576XHD Polypropylene Homopolymer, Film Grade Low Residuals TOTAL Polypropylene 3576XHD utilizes the new ATOFINA proprietary process technology to provide extremely low residuals for improved color stability and clarity.Antiblock. 3576XHD is .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPH 3764 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics and Multifilament Yarns Process Stability TOTAL Petrochemicals Polypropylene 3764 features excellent processability and gas fade resistance.FDA. 3764 complies with all applicable FDA regulations for food contact applicat.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPH 3866 Polypropylene, Controlled Rheology Grade Homopolymer for Spunbond Nonwoven Fabrics, Multifilament Yarns, and Extrusion Coating Process Stability TOTAL Petrochemicals Polypropylene 3866 features excellent processability and gas fade resistance.FDA. 3866 complies with all applicable FDA regulations for food contact applicat.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming This grade belongs to the Total Ecosolution line.Polypropylene PPH 4026 is a polypropylene homopolymer specifically developed to offer outstanding processability for sheet extrusion and thermoformin.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 3045 Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 11642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 60 g/10 min.Polypropylene PPC 11642 is characterized by high fluidity with good mechanical prope.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ISO 1183 |
Total PPC 11812 S01 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11812 S01 has been developed for high speed injection molding of thin walled packaging containers requiring top level impact resistance at cold temperature (-20°C). It is charact.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4820WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, h.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4920WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4920WZ is a nucleated impact copolymer with a Melt Flow index of 105 g/10 min.TOTAL Polypropylene 4920WZ is characterized by excellent stiffness and impact resista.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D1505 |
Total PPC 4944CWZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4944CWZ is a nucleated and controlled rheology impact copolymer with a very high Melt Flow index of 50 g/10 min.TOTAL 4944CWZ is characterized by improved stiffnes.. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
Braskem H 155 Fiber Extrusion Polypropylene Homopolymer Meltblown nonwoven applications for hygienic, medical and hospital disposable devices; Filters and oil adsorbents.Information provided by Braskem. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
Braskem H 203 Fiber Extrusion Polypropylene Homopolymer Continuous filaments for carpets, sewing yarns and ropes; Staple fibers for rugs and blankets; Nonwovens by thermobonded process.Information provided by Braskem. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
Braskem H 604 Thermoforming & Extrusion Polypropylene Homopolymer Transparent packaging for food; Flat and corrugated sheets for school and office folders.Information provided by Braskem. |
|||
Specific Gravity | 0.905 g/cc | 0.905 g/cc | ASTM D792 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |