A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman SCHULAMID® 66 MV3 Unreinforced Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 3.175 mm
0.015 in/in

@Thickness 0.1250 in
ASTM D955
Mechanical Properties Metric English Comments
Flexural Strength 107.8 MPa
15640 psi
ASTM D790
Flexural Modulus 2.977 GPa
431.8 ksi
ASTM D970
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 188 °C
371 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Melt Temperature 280 - 305 °C
536 - 581 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Drying Temperature 79.4 °C
175 °F
Dry Time 2 - 4 hour
2 - 4 hour
Predrying