Material Notes:
EP LS, “Powered by Reactamine® Technology”, is a special MDI prepolymer designed to be pumped into voids or walls. EP LS reacts with water to create a shaving cream-like foam. This foam will solidify in minutes, stopping the leak and filing the void. Caution should be taken to ensure that only the correct amount of EP LS should be used. Excess could create too much pressure. Special check valves are generally used to prevent the foam from extruding out the entrance hole. It has a functionality of 2. EP LS contains 16% NCO.Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Density 0.0160 g/cc
0.000579 lb/in³
Free Rise Density, 5% H<sub>2</sub>O
0.0240 g/cc
0.000868 lb/in³
Free Rise Density, 4% H<sub>2</sub>O
0.0320 g/cc
0.00116 lb/in³
Free Rise Density, 3% H<sub>2</sub>O
0.0481 g/cc
0.00174 lb/in³
Free Rise Density, 2% H<sub>2</sub>O
0.0801 g/cc
0.00289 lb/in³
Free Rise Density, 1% H<sub>2</sub>O
Viscosity 1000 cP

@Temperature 75.0 °C
1000 cP

@Temperature 167 °F
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 0.000 °C
32.0 °F