ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an excellent choice for the molding of intricate patterns, skin molding or for applications where lower modulus and extremely tough rubber are required. A variety of catalysts are offered with this material. Complies with FDA indirect food contact regulation CFR 177.2600 when used with QM Cat Clear FG. Refer to QM Cat Clear FG data sheet for typical properties. Key Features:Low ViscosityHigh tear strengthFast demold time Low modulusMain Applications: Molds for small statues, large statues Molds for polyester, polyurethane and epoxy resin castings Molds for technical articles and prototypes Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Uncatalyzed, QM CAT RED 3
1.00 g/cc
1.00 g/cc
Uncatalyzed, QM CAT BLUE
1.00 g/cc
1.00 g/cc
Uncatalyzed, QM CAT PURPLE
1.23 g/cc
1.23 g/cc
catalyzed with QM CAT PURPLE
1.23 g/cc
1.23 g/cc
catalyzed with QM CAT RED 3
1.23 g/cc
1.23 g/cc
catalyzed with QM CAT BLUE
1.25 g/cc
1.25 g/cc
Base
Viscosity 100 cP
100 cP
Uncatalyzed, QM CAT RED 3
100 cP
100 cP
Uncatalyzed, QM CAT BLUE
100 cP
100 cP
Uncatalyzed, QM CAT PURPLE
12000 cP
12000 cP
catalyzed with QM CAT BLUE
12000 cP
12000 cP
catalyzed with QM CAT RED 3
12000 cP
12000 cP
catalyzed with QM CAT PURPLE
15000 cP
15000 cP
Base
Linear Mold Shrinkage <= 0.0030 cm/cm

@Temperature 25.0 °C,
Time 259000 sec
<= 0.0030 in/in

@Temperature 77.0 °F,
Time 72.0 hour
Cured
Storage Temperature <= 38.0 °C
<= 100 °F
6 months
Mechanical Properties Metric English Comments
Hardness, Shore A 14
14
cured 72 hrs@ RT
Tensile Strength, Yield 2.75 MPa
399 psi
cured 72 hrs@ RT
Elongation at Break 500 %
500 %
cured 72 hrs@ RT
Tear Strength 19.3 kN/m
110 pli
cured 72 hrs@ RT
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Processing Properties Metric English Comments
Dry Time 4 - 6 hour
4 - 6 hour
Demold time, catalyzed with QM CAT RED 3
12 - 16 hour
12 - 16 hour
Demold time, catalyzed with QM CAT PURPLE
16 - 24 hour
16 - 24 hour
Demold time, catalyzed with QM CAT BLUE
Cure Time 45.0 - 60.0 min
0.750 - 1.00 hour
Tack Free Time, catalyzed with QM CAT RED 3
240 - 360 min
4.00 - 6.00 hour
Tack Free Time, catalyzed with QM CAT PURPLE
360 - 480 min
6.00 - 8.00 hour
Tack Free Time, catalyzed with QM cat BLUE
Descriptive Properties Value Comments
Color Beige
Base
Blue
Uncatalyzed, QM CAT BLUE
Light Blue
catalyzed with QM CAT BLUE
Light Purple
catalyzed with QM CAT PURPLE
Light Red
catalyzed with QM CAT RED 3
Purple
Uncatalyzed, QM CAT PURPLE
Red
Uncatalyzed, QM CAT RED 3
Work Life 25 mins
catalyzed with QM CAT PURPLE
45 mins
catalyzed with QM CAT BLUE
7 mins
catalyzed with QM CAT RED 3
Users viewing this material also viewed the following: