Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A.D. Compound Adene NCZAG Copolymer 70% CaCO3 Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer A.D. Compound
Trade Name Adene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A.D. Compound Adene NCZAG Copolymer 70% CaCO3 Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A.D. Compound
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Filler Content 70 %
70 %
ISO 3451 / 1
Melt Index of Compound 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ISO 868
Tensile Strength, Yield 13.0 MPa
1890 psi
ISO 527
Elongation at Break 25 %
25 %
ISO 527
Elongation at Yield 3.0 %
3.0 %
ISO 527
Flexural Modulus 3.50 GPa
508 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180/1A
Izod Impact, Unnotched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75
Vicat Softening Point 85.0 °C
185 °F
49 N; ISO 306
Copyright © lookpolymers.com All Rights Reserved