Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A.D. Compound Adene NTFAG Copolymer 20% Talc Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer A.D. Compound
Trade Name Adene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A.D. Compound Adene NTFAG Copolymer 20% Talc Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A.D. Compound
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Filler Content 20 %
20 %
ISO 3451 / 1
Melt Index of Compound 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ISO 868
Tensile Strength, Yield 22.0 MPa
3190 psi
ISO 527
Elongation at Break 65 %
65 %
ISO 527
Elongation at Yield 9.0 %
9.0 %
ISO 527
Flexural Modulus 1.75 GPa
254 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75
Vicat Softening Point 70.0 °C
158 °F
49 N; ISO 306
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved