Material Notes:
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then naturally aged.
Physical Properties Metric English Comments
Density 2.801 g/cc
0.1012 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell >= 105
>= 105
Tensile Strength, Ultimate 370 - 390 MPa
53700 - 56600 psi
Rm
Tensile Strength, Yield >= 240 MPa

@Strain 0.200 %
>= 34800 psi

@Strain 0.200 %
Elongation at Break <= 15 %
<= 15 %
Modulus of Elasticity 70.0 GPa
10200 ksi
Thermal Properties Metric English Comments
CTE, linear 23.0 µm/m-°C

@Temperature 20.0 °C
12.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 130.0 - 200.0 W/m-K
902.2 - 1388 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000357 - 0.00000556 ohm-cm
0.00000357 - 0.00000556 ohm-cm
Descriptive Properties Value Comments
Corrosion Resistance Sufficient
Machinability Good
Protective Anodizing Good, not decorative
Welding Properties (WIG, MIG) Less Suitable
Users viewing this material also viewed the following: