Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ATI Allvac® Astroloy Nickel Superalloy, Heat Treatment: 1163°C (2125°F) + Age

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer ATI Allvac
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Astroloy Nickel Superalloy, Heat Treatment: 1163°C (2125°F) + Age.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Discs, rings, bolts for gas turbines.
Physical Properties Metric English Comments
Density 7.91 g/cc
0.286 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 369
369
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 403
403
Estimated from Rockwell C value.
Hardness, Rockwell C 40
40
Hardness, Vickers 386
386
Estimated from Rockwell C value.
Tensile Strength, Ultimate 1241 MPa
180000 psi
Tensile Strength, Yield 862 MPa

@Strain 0.200 %
125000 psi

@Strain 0.200 %
Elongation at Break 12 %
12 %
Reduction of Area 11 %
11 %
Component Elements Properties Metric English Comments
Aluminum, Al 4.0 %
4.0 %
Boron, B 0.025 %
0.025 %
Carbon, C 0.040 %
0.040 %
Chromium, Cr 15 %
15 %
Cobalt, Co 17 %
17 %
Molybdenum, Mo 5.0 %
5.0 %
Nickel, Ni 55 %
55 %
as balance
Titanium, Ti 3.5 %
3.5 %