Physical Properties Metric English Comments
Density 7.92 g/cc
0.286 lb/in³
Sintered
Kinetics MIM 316 Stainless Steel (Premium Grade)
Austenitic stainless steel. Excellent corrosion resistance. Excellent elongation. Non-magnetic. Easily weldable. Can be polished to a mirror finish. Provides better elongation and ductility over the..
Density 7.92 g/cc
0.286 lb/in³
Latrobe DuraTechâ„¢ M4 High Carbon Powder Metal High Speed Steel (ASTM M4)
DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v..
Density 7.92 g/cc
0.286 lb/in³
Latrobe DuraTechâ„¢ M4 Powder Metal High Speed Steel (ASTM M4)
DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v..
Density 7.93 g/cc
0.286 lb/in³
Special Metals BRIGHTRAY® Alloy 35 Electrical Resistance Alloy
A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 1920°F (1050°C). It is similar to BRIGHTRAY alloy F but with rare-earth additions for greater resist..
Density 7.92 g/cc
0.286 lb/in³
Special Metals UDIMET® Alloy 250 Maraging Steel
A high-strength, maraging steel of iron and nickel with additions of molybdenum and titanium. It has the strength of standard 18Ni (250) maraging steel but the advantages of containing less molybde..
Density 7.93 g/cc
0.286 lb/in³
Wall Colmonoy COLMONOY® 6 PTA Nickel-Base Hard Surfacing Alloy With Chromium Boride
Description: Optimized formulation to offset dilution and alloy loss from the arc. Designed for PTA Application.Applications: Colmonoy 6 PTA is designed for plasma transferred arc (PTA) application...
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 305 Austenitic Stainless Steel, 1/2 Hardened
Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. ..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 305 Austenitic Stainless Steel, 1/4 Hardened
Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. ..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 305 Austenitic Stainless Steel, Annealed
Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. ..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316 Austenitic Stainless Steel, 1/2 Hardened
The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 ..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316 Austenitic Stainless Steel, 1/4 Hardened
The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 ..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316 Austenitic Stainless Steel, 1/8 Hardened
The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 ..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316 Austenitic Stainless Steel, 3/4 Hardened
The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 ..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316 Austenitic Stainless Steel, Annealed
The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 ..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316 Austenitic Stainless Steel, Full Hardened
The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 ..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316L Austenitic Stainless Steel, 1/2 Hardened
Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316L Austenitic Stainless Steel, 1/4 Hardened
Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316L Austenitic Stainless Steel, 1/8 Hardened
Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316L Austenitic Stainless Steel, 3/4 Hardened
Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316L Austenitic Stainless Steel, Annealed
Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a..
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Eagle Brass 316L Austenitic Stainless Steel, Full Hardened
Type 316L is an extra-low carbon version of Type 316 that minimizes carbide precipitation. Typical uses include exhaust manifolds, furnace parts, heat exchangers, jet engine parts, pharmaceutical a..
Density 7.92 g/cc
0.286 lb/in³
Crucible Steel REX® M4 High Speed Steel
REX M4 is a special purpose high speed steel designed to give high wear resistance in tools. Its high vanadium and carbon content provide for high resistance to cratering and wear in cold work punch..
Density 7.92 g/cc
0.286 lb/in³
Crucible Steel REX® TMO High Speed Steel, AISI M1
REX TMO molybdenum-tungsten high speed steel is a tough general purpose high speed steel with high cutting efficiency and excellent finishing properties. It is adapted to fast light cuts on soft or ..
Density 7.92 g/cc
0.286 lb/in³
soft annealed
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel
Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W ..
Density 7.91 g/cc
0.286 lb/in³
ATI Allvac® Astroloy Nickel Superalloy, Heat Treatment: 1163°C (2125°F) + Age
Data provided by Allvac.Applications: Discs, rings, bolts for gas turbines.
Density 7.92 g/cc
0.286 lb/in³
ATI Allvac® Nickelvac® A-286 Specialty Steel, Heat Treatment: 982°C (1800°F) + Age
Data provided by Allvac.Applications: Jet engines, superchargers, missile components, fasteners, cryogenic equipment, nuclear, corrosive deep well hardware.
Density 7.92 g/cc
0.286 lb/in³
Solution Treated
ATI Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286
Allegheny Ludlum Altemp A286 alloy is an iron-base superalloy useful for applications requiring high strength and corrosion resistance up to 704 degrees Celsius and for lower stress applications at ..
Density 7.93 g/cc
0.286 lb/in³
RT
Outokumpu 4948 High Temperature Austenitic Stainless Steel
Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for..
Density 7.92 g/cc
0.286 lb/in³
ATI Allegheny Ludlum Stainless Steel Type 321 (UNS S32100)
AL 321 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°..