ATI Allvac® Vasco® D6AC Specialty Steel, Heat Treatment: 913°C (1675°F) Q+T

Category Metal , Ferrous Metal
Manufacturer ATI Allvac
Trade Name Vasco®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Vasco® D6AC Specialty Steel, Heat Treatment: 913°C (1675°F) Q+T.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: High performance aircraft structural parts.
Physical Properties Metric English Comments
Density 7.78 g/cc
0.281 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 422
422
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 463
463
Estimated from Rockwell C value.
Hardness, Rockwell C 45
45
Hardness, Vickers 442
442
Estimated from Rockwell C value.
Tensile Strength, Ultimate 1483 MPa
215100 psi
Tensile Strength, Yield 1379 MPa

@Strain 0.200 %
200000 psi

@Strain 0.200 %
Elongation at Break 12 %
12 %
Reduction of Area 40 %
40 %
Component Elements Properties Metric English Comments
Carbon, C 0.48 %
0.48 %
Chromium, Cr 1.1 %
1.1 %
Iron, Fe 96 %
96 %
as balance
Manganese, Mn 0.80 %
0.80 %
Molybdenum, Mo 1.0 %
1.0 %
Nickel, Ni 0.60 %
0.60 %
Phosphorous, P 0.0050 %
0.0050 %
Silicon, Si 0.23 %
0.23 %
Sulfur, S 0.0050 %
0.0050 %
Vanadium, V 0.12 %
0.12 %