Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROPRENE® GFABS 4020 Glass Filled Acrylonitrile-Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® GFABS 4020 Glass Filled Acrylonitrile-Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROPRENE® GFABS 4000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Filler Content 20 %
20 %
Glass; ASTM D2584
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Melt Flow 5.0 - 10 g/10 min
5.0 - 10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 75.8 MPa
11000 psi
ASTM D638
Flexural Modulus 5.62 GPa
815 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Users viewing this material also viewed the following: