Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 50-3/AboCure 50-3 Clear Epoxy Adhesive and Casting Compound

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 50-3/AboCure 50-3 Clear Epoxy Adhesive and Casting Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboCast 50-3 is a medium viscosity, clear Epoxy Resin. AboCure 50-3 is clear-amber in color, room-temperature-cure, and slow. It has variable ratios and low viscosity. AboCast 50-3/AboCure 50-3 is used for casting, potting, and encapsulating applications where bubble-free flow, high resistivity, and low exotherm are needed simultaneously.
Physical Properties Metric English Comments
Water Absorption 0.49 %

@Time 605000 sec
0.49 %

@Time 168 hour
Viscosity 2500 cP
2500 cP
Mechanical Properties Metric English Comments
Tensile Strength at Break 59.3 MPa
8600 psi
Elongation at Break 6.0 %
6.0 %
Compressive Strength 77.9 MPa
11300 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 72.0 °C
162 °F
Deflection Temp at unknown load
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
Processing Properties Metric English Comments
Pot Life 180 min
180 min
Descriptive Properties Value Comments
Hardening Time (min) 720
Parts by Weight (pbw) 100
AboCast 50-3
40
AboCure 50-3