Material Notes:
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applications include: bonding, laminating, casting, embedding, electrical potting, impregnating, coating, etc. It can be supplied in several variations to modify viscosity, reaction rate, color, most physical and chemical properties, and with many fillers to meet most requirements.
Physical Properties Metric English Comments
Water Absorption 2.4 %

@Time 2.59e+6 sec
2.4 %

@Time 720 hour
immersion; cured 3 hours @ 100°C
Viscosity 2650 cP
2650 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 80

@Temperature 25.0 °C
80

@Temperature 77.0 °F
cured 2 hrs. @ 93°C
86

@Temperature 0.000 °C
86

@Temperature 32.0 °F
cured 2 hrs. @ 93°C
90

@Temperature -60.0 °C
90

@Temperature -76.0 °F
cured 2 hrs. @ 93°C
Tensile Strength, Ultimate 41.7 MPa
6050 psi
cured 2 hours @ 93°C
61.4 MPa
8900 psi
cured 8 hours @ 93°C
Elongation at Break 14 %
14 %
cured 8 hours @ 93°C
21 %
21 %
cured 2 hours @ 93°C
Electrical Properties Metric English Comments
Volume Resistivity 2.50e+13 ohm-cm

@Temperature 100 °C
2.50e+13 ohm-cm

@Temperature 212 °F
cured 2 hours @ 93°C
4.80e+15 ohm-cm

@Temperature 25.0 °C
4.80e+15 ohm-cm

@Temperature 77.0 °F
cured 2 hours @ 93°C
Processing Properties Metric English Comments
Pot Life 180 min

@Temperature 25.0 °C
180 min

@Temperature 77.0 °F
200 g
Descriptive Properties Value Comments
Parts by Weight (pbw) 100
AboCast 8110-9
43
AboCure 50-1