Abatron AboCast/AboCure 50-7/8501-4 High Temperature Resistant Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced , Epoxy, High Temperature
Manufacturer Abatron
Trade Name AboCast/AboCure
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast/AboCure 50-7/8501-4 High Temperature Resistant Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clear amber, high viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to be used at temperatures up to 300°C. Casting and assembly of tools, patterns, models and structural components that must operate in extremely hot and corrosive environments.Processing: 100/89 ratio (pbw). Cured 2 hours at 95°C + 24 hour post-cure at 260°C. Information provided by Abatron.
Physical Properties Metric English Comments
Viscosity 150 cP

@Temperature 80.0 °C
150 cP

@Temperature 176 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 49.0 MPa
7100 psi
Lower curing cycle, lower heat resistance
Flexural Strength 101 MPa
14600 psi
Lower curing cycle, lower heat resistance
Compressive Strength 256 MPa
37100 psi
Lower curing cycle, lower heat resistance
Thermal Properties Metric English Comments
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 298 °C
568 °F
Processing Properties Metric English Comments
Pot Life 120 min

@Temperature 80.0 °C
120 min

@Temperature 176 °F