Abatron Epotron 5 Clear Liquid Epoxy Adhesive for Structural Bonding

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Abatron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron Epotron 5 Clear Liquid Epoxy Adhesive for Structural Bonding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Epotron 5 is a clear liquid epoxy adhesive for structural bonding. It is recommended for high-strength, permanent bonding of metal, ceramic, glass, laminates, and most rigid materials. Features: High Compressive Strength; High Tensile Strength; High Impact Resistance; Contains no VOC's or Water; Hardens Slowly; Variable Ratio; Bonds to Virtually All Rigid Surfaces; Structural; Transparent Liquid; and 2-Component. Benefits: Tenacious Adhesion; Safe and Easy to Use; Permanent; Multiple Uses. Epotron 5 is used for bonding, laminating, and repairing virtually all rigid surfaces such as wood, stone, concrete, masonry, metal, ceramics, glass, wood, and fiberglass. It is used for repairs in factories, warehouses, office buildings, homes, and shops, both indoors and outdoors. Epotron 5 can be applied in any thickness needed, and it fully resists shrinkage. It can be applied with a brush, applicator bottle, trowel, or squeegee.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Volatiles 0.00 %
0.00 %
EPA method #24
Viscosity 180 cP
180 cP
ASTM-D562
Mechanical Properties Metric English Comments
Tensile Strength at Break 57.2 MPa
8300 psi
ASTM-D638
Elongation at Break 4.8 %
4.8 %
ASTM-D638
Flexural Strength 65.8 MPa
9550 psi
ASTM-D790
Compressive Strength 85.15 MPa
12350 psi
ASTM-D695
Adhesive Bond Strength 10.89 MPa
1579 psi
ASTM-D4541
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
ASTM-D2485
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Cure Time 5760 - 7200 min
96.0 - 120 hour
(4-5 Days)
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Impact Resistance 80
ASTM-D4226
Induction Period (min) 5 to 10
Parts by Weight (pbw) 100
Part A Resin
35-100
Part B Hardener
Tack-free Time (min) 240