Mechanical Properties Metric English Comments
Tensile Strength at Break 57.2 MPa
8300 psi
ASTM D638
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant
Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
Tensile Strength at Break 57.2 MPa
8300 psi
ASTM D638
Polymer Resources TP-FR2-[color]-WR Polybutylene Terephthalate, Flame Retardant, Wear Resistant
Polybutylene Terephthalate, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Tensile Strength at Break 57.2 MPa
8300 psi
ASTM D638
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate
Information provided by Ravago.
Tensile Strength at Break 57.2 MPa
8300 psi
ASTM D638
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate
Information provided by Ravago.
Tensile Strength at Break 57.2 MPa
8300 psi
chs 20 in/min; ASTM D412
Diamond Polymers Softflex® 6538 Thermoplastic Elastomer Alloy, Clear
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength at Break 57.2 MPa
8300 psi
ASTM-D638
Abatron Epotron 5 Clear Liquid Epoxy Adhesive for Structural Bonding
Epotron 5 is a clear liquid epoxy adhesive for structural bonding. It is recommended for high-strength, permanent bonding of metal, ceramic, glass, laminates, and most rigid materials. Features: Hi..
Tensile Strength at Break 57.2 - 71.0 MPa
8300 - 10300 psi
Bulk Molding Compounds BMC A50-XHS Bulk molding compound
Description: BMC A50­XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in pre­weighted slugs. Due to the excellent flow and controlled reactivity, BMC A50­XHS i..
Tensile Strength at Break 57.2 - 71.0 MPa
8300 - 10300 psi
Bulk Molding Compounds BMC A50-XHS-U Bulk molding compound
Description: BMC A50-XHS-U is a high strength bulk molding compound with a UL F1 rating for outdoor exposure. This material was specifically designed for outdoor lighting and electrical applications..