Material Notes:
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
MD; ASTM D955
Melt Flow 1.8 g/10 min
1.8 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength at Break 35.0 MPa
5080 psi
ASTM D638
Tensile Strength, Yield 54.0 MPa
7830 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 1.80 GPa
261 ksi
ASTM D638
Flexural Strength 75.01 MPa
10880 psi
ASTM D790
Flexural Modulus 2.699 GPa
391.5 ksi
ASTM D790
Izod Impact, Notched 3.10 J/cm
5.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.1 °C
169 °F
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in
UL File #E56070