Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Copolymer CP0436W40L1 Wollastonite Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0436W40L1 Wollastonite Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
MD; ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Ash 40 %
40 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 45
45
ASTM D785
Tensile Strength at Break 16.0 MPa
2320 psi
ASTM D638
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Tensile Modulus 3.00 GPa
435 ksi
ASTM D638
Flexural Strength 27.0 MPa
3920 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
Users viewing this material also viewed the following: