Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Homopolymer HP0334T20L1 Talc Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0334T20L1 Talc Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.038 g/cc
0.03750 lb/in³
ASTM D792
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
MD; ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Ash 20 %
20 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 92
92
ASTM D785
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Break 16 %
16 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 1.700 GPa
246.5 ksi
ASTM D638
Flexural Strength 47.0 MPa
6820 psi
ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
ASTM D790
Izod Impact, Notched 0.352 J/cm
0.660 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 122 °C
252 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F