Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Bead Filled , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer Addiplast
Trade Name Addinyl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, 30% glass bead filled, with halogensInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 89
89
Conditioned; ISO 868
90
90
ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
Conditioned; ISO R 527
55.0 MPa
7980 psi
ISO R 527
Elongation at Break 3.0 %
3.0 %
ISO R 527
7.0 %
7.0 %
Conditioned; ISO R 527
Modulus of Elasticity 2.40 GPa
348 ksi
Conditioned; ISO 178
4.80 GPa
696 ksi
ISO 178
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
Conditioned; ISO 180/1A
3.00 kJ/m²
1.43 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/IeU
2.20 J/cm²
10.5 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179/IeA
0.200 J/cm²
0.952 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
ISO 75-2/AF
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Oxygen Index 31 %
31 %
ISO 4589
Glow Wire Test 960 °C
1760 °F
CEI 60695/2/1
Electrical Properties Metric English Comments
Comparative Tracking Index 275 V
275 V
CEI 60112/Solution A