Addiplast Addinyl B2I V25 Flame Retardant Nylon 6, 25% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer Addiplast
Trade Name Addinyl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addinyl B2I V25 Flame Retardant Nylon 6, 25% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, 25% glass fiber reinforced, halogen freeInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
Conditioned; ISO 868
88
88
ISO 868
Tensile Strength at Break 80.0 MPa
11600 psi
Conditioned; ISO R 527
120 MPa
17400 psi
ISO R 527
Elongation at Break 5.0 %
5.0 %
ISO R 527
7.0 %
7.0 %
Conditioned; ISO R 527
Modulus of Elasticity 5.00 GPa
725 ksi
Conditioned; ISO 178
7.50 GPa
1090 ksi
ISO 178
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180/1A
13.0 kJ/m²
6.19 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched 6.20 J/cm²
29.5 ft-lb/in²
ISO 179/IeU
6.20 J/cm²
29.5 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/IeA
1.20 J/cm²
5.71 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-2/AF
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Oxygen Index 31 %
31 %
ISO 4589
Glow Wire Test 960 °C
1760 °F
CEI 60695/2/1
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A